Laser Micro-Machining & Polishing

picture

· 

   Process

   o  LaserCutting 

 Laser beam kerf width varies with alloy,thickness,and velocity of process. A typical range is
    20microns (0.0008") to 100microns (0.004"). We recommend planning on a kerf of 30microns
    (0.0012") if your part can accommodate it.

 Peiertech recommends setting tolerance of +/- 15microns (0.0006") for laser-cut parts and
    +/- 20microns (0.0008") for laser-cut and electropolished parts. Contact us with other requirements.

      •   o  Polishing: 

      •  Material removal typically ranges from 0.005mm (0.0002″) to 0.075mm (0.003″) total
            Dimensional reduction.

      •  Material removal can also be specified in mass removal.

      •  Dimensional removal is generally equivalent in thickness and width, but there are exceptions.

      •  We provide the following surface treatment based on the customer’s requirements:

        •         -Electropolishing

        •         -Mechanical polishing

        •         -Microabrasive blasting

        •         -Chemical cleaning

Peiertech provides
• Nitinol materials,
• Tubular laser micro-machining& post-processing, and
• Precision assembly contract manufacturing to the medical deviceindustry worldwide.